Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® Advanced N3HG6 LT BK - PA9T-GF30 - BASF

Material Data Center offers the following functions for Ultramid® Advanced N3HG6 LT BK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Partially aromatic, glassfiber reinforced polyphthalamide for injection molding with strong mechanical properties especially at elevated temperatures, good long-term thermal stability and outstanding chemical resistance for highly stressed parts.
Ultramid® Advanced N3HG6 LT BK can be characterized as compound with high toughness, stiffness, extremely low water absorption and outstanding dimensional stability. It features high flowability and allows filling of complex parts with thin wall thickness. Ultramid® Advanced N3HG6 LT BK is easily processable with excellent melt stability.

Markets & applications
Automotive: Fuel system, cooling system, powertrain, Auto E&E, sensors, pumps, fuel cell
E&E: Connectors
Consumer goods: Home appliances, consumer electronics
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.5 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.0 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 10000 / - MPa ISO 527
Stress at break 185 / - MPa ISO 527
Strain at break 2.4 / - % ISO 527
Charpy impact strength, +23°C 60 / - kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 55 / - kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 8 / - kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 7 / - kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 300 / * °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 120 / * °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 270 / * °C ISO 75-1/-2
Other propertiesdry / condUnitTest Standard
Density 1370 / - kg/m³ ISO 1183
Bulk density 700 kg/m³ -
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 330 °C ISO 294
Injection Molding, mold temperature 140 °C ISO 294
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 120 °C -
Pre-drying - Time 8 h -
Processing humidity ≤0.05 % -
Melt temperature 320 - 340 °C -
Mold temperature 125 - 170 °C -
Processing Recommendation ExtrusionValueUnitTest Standard
Melt temperature 320 - 340 °C -
Diagrams
Stress-strain , Ultramid® Advanced N3HG6 LT BK (dry), PA9T-GF30, BASF
Stress-strain , Ultramid® Advanced N3HG6 LT BK (cond.), PA9T-GF30, BASF
Secant modulus-strain , Ultramid® Advanced N3HG6 LT BK (dry), PA9T-GF30, BASF
Secant modulus-strain , Ultramid® Advanced N3HG6 LT BK (cond.), PA9T-GF30, BASF
Tensile modulus-temperature , Ultramid® Advanced N3HG6 LT BK (dry), PA9T-GF30, BASF
Tensile modulus-temperature , Ultramid® Advanced N3HG6 LT BK (cond.), PA9T-GF30, BASF
Characteristics
Processing
Injection Molding, Other Extrusion
Delivery form
Pellets, Black
Special Characteristics
Heat stabilized or stable to heat
Features
Thermal Stability
Chemical Resistance
General Chemical Resistance
Applications
Automotive, Electrical and Electronical
Regional Availability
Other text information
Injection molding
PREPROCESSING
Pre/Post-processing, max. allowed water content: .05 %
Pre/Post-processing, Pre-drying, Temperature: 120 °C
Pre/Post-processing, Pre-drying, Time: 8 h

PROCESSING
injection molding, Melt temperature, range: 320 - 340 °C
injection molding, Melt temperature, recommended: 330 °C
injection molding, Mold temperature, range: 125 - 170 °C
injection molding, Mold temperature, recommended: 140 °C
injection molding, Dwell time, thermoplastics: 5 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com